Czasopisma
Czasopisma
Czasopisma
ATEST - OCHRONA PRACY
ATEST - OCHRONA PRACY
AURA
AURA
AUTO MOTO SERWIS
AUTO MOTO SERWIS
CHEMIK
CHEMIK
CHŁODNICTWO
CHŁODNICTWO
CIEPŁOWNICTWO, OGRZEWNICTWO, WENTYLACJA
CIEPŁOWNICTWO, OGRZEWNICTWO, WENTYLACJA
DOZÓR TECHNICZNY
DOZÓR TECHNICZNY
ELEKTROINSTALATOR
ELEKTROINSTALATOR
ELEKTRONIKA - KONSTRUKCJE, TECHNOLOGIE, ZASTOSOWANIA
ELEKTRONIKA - KONSTRUKCJE, TECHNOLOGIE, ZASTOSOWANIA
Czasopisma
Czasopisma
Czasopisma
GAZETA CUKROWNICZA
GAZETA CUKROWNICZA
GAZ, WODA I TECHNIKA SANITARNA
GAZ, WODA I TECHNIKA SANITARNA
GOSPODARKA MIĘSNA
GOSPODARKA MIĘSNA
GOSPODARKA WODNA
GOSPODARKA WODNA
HUTNIK - WIADOMOŚCI HUTNICZE
HUTNIK - WIADOMOŚCI HUTNICZE
INŻYNIERIA MATERIAŁOWA
INŻYNIERIA MATERIAŁOWA
MASZYNY, TECHNOLOGIE, MATERIAŁY - TECHNIKA ZAGRANICZNA
MASZYNY, TECHNOLOGIE, MATERIAŁY - TECHNIKA ZAGRANICZNA
MATERIAŁY BUDOWLANE
MATERIAŁY BUDOWLANE
OCHRONA PRZED KOROZJĄ
OCHRONA PRZED KOROZJĄ
ODZIEŻ
ODZIEŻ
Czasopisma
Czasopisma
Czasopisma
OPAKOWANIE
OPAKOWANIE
PACKAGING REVIEW
PACKAGING REVIEW
POLISH TECHNICAL REVIEW
POLISH TECHNICAL REVIEW
PROBLEMY JAKOŚCI
PROBLEMY JAKOŚCI
PRZEGLĄD ELEKTROTECHNICZNY
PRZEGLĄD ELEKTROTECHNICZNY
PRZEGLĄD GASTRONOMICZNY
PRZEGLĄD GASTRONOMICZNY
PRZEGLĄD GEODEZYJNY
PRZEGLĄD GEODEZYJNY
PRZEGLĄD MECHANICZNY
PRZEGLĄD MECHANICZNY
PRZEGLĄD PAPIERNICZY
PRZEGLĄD PAPIERNICZY
PRZEGLĄD PIEKARSKI I CUKIERNICZY
PRZEGLĄD PIEKARSKI I CUKIERNICZY
Czasopisma
Czasopisma
Czasopisma
PRZEGLĄD TECHNICZNY. GAZETA INŻYNIERSKA
PRZEGLĄD TECHNICZNY. GAZETA INŻYNIERSKA
PRZEGLĄD TELEKOMUNIKACYJNY - WIADOMOŚCI TELEKOMUNIKACYJNE
PRZEGLĄD TELEKOMUNIKACYJNY - WIADOMOŚCI TELEKOMUNIKACYJNE
PRZEGLĄD WŁÓKIENNICZY - WŁÓKNO, ODZIEŻ, SKÓRA
PRZEGLĄD WŁÓKIENNICZY - WŁÓKNO, ODZIEŻ, SKÓRA
PRZEGLĄD ZBOŻOWO-MŁYNARSKI
PRZEGLĄD ZBOŻOWO-MŁYNARSKI
PRZEMYSŁ CHEMICZNY
PRZEMYSŁ CHEMICZNY
PRZEMYSŁ FERMENTACYJNY I OWOCOWO-WARZYWNY
PRZEMYSŁ FERMENTACYJNY I OWOCOWO-WARZYWNY
PRZEMYSŁ SPOŻYWCZY
PRZEMYSŁ SPOŻYWCZY
RUDY I METALE NIEŻELAZNE
RUDY I METALE NIEŻELAZNE
SZKŁO I CERAMIKA
SZKŁO I CERAMIKA
TECHNOLOGIA I AUTOMATYZACJA MONTAŻU
TECHNOLOGIA I AUTOMATYZACJA MONTAŻU
WIADOMOŚCI ELEKTROTECHNICZNE
WIADOMOŚCI ELEKTROTECHNICZNE
WOKÓŁ PŁYTEK CERAMICZNYCH
WOKÓŁ PŁYTEK CERAMICZNYCH
Menu
Menu
Menu
Prenumerata
Prenumerata
Publikacje
Publikacje
Drukarnia
Drukarnia
Kolportaż
Kolportaż
Reklama
Reklama
O nas
O nas
ui-button
Twój Koszyk
Twój koszyk jest pusty.
Niezalogowany
Niezalogowany
Zaloguj się
Zarejestruj się
Reset hasła
Czasopismo
|
PRZEMYSŁ CHEMICZNY
|
Rocznik 2018 - zeszyt 8
Skład chemiczny i mikrostruktura biowęgli otrzymanych pirolitycznie z odpadów roślinnych
The chemical composition and microstructure of biocarbons received by pyrolysis from vegetable waste
10.15199/62.2018.8.29
Jarosław Molenda
Marek Swat
Marek Wolszczak
nr katalogowy: 115529
10.15199/62.2018.8.29
Streszczenie
Celem badań była ocena możliwości otrzymania biowęgli z aktywnymi grupami funkcyjnymi podczas jednoetapowej pirolizy odpadów roślinnych, tj. słomy pszenicznej, odpadów kukurydzianych, paździerzy lnianych i pestek wiśni, a także charakterystyka mikrostruktury powstałych karbonizatów. Próbki biowęgli otrzymano podczas laboratoryjnej pirolizy w atmosferze ditlenku węgla, stosując kaskadowe ogrzewanie do 500°C, a następnie poddano je badaniom za pomocą SEM/EDS oraz FTIR. Zastosowane warunki pirolizy pozwalają na otrzymanie w jednoetapowym procesie biowęgli, zawierających tlenowe i azotowe ugrupowania strukturalne, które mogą stanowić centra aktywności szczególnie przydatne podczas sorpcji. Piroliza powoduje zmiany w mikrostrukturze przetwarzanych termicznie pestek wiśni oraz odpadów kukurydzianych, a paździerze lniane i słoma pszeniczna poddane pirolizie zachowują swoją włóknistą mikrostrukturę.
Abstract
Wheat straw, flax harl, corn waste (stems and leaves) and cherry seeds were heated to 500°C in a CO2 atm. (95 min, gas flow 5 L/min) and then the carbonizates were analyzed by scanning electron microscopy coupled with X-ray microanal. and Fourier transform ir spectroscopy. The pyrolysis resulted in an increase in the C and N content as well as a decrease in the O content for all types biocarbons and also changes in the microstructure of thermally transformed cherry seeds and corn waste, while wheat straw and flax harl, previously subjected to pyrolysis, kept their firbrous microstructure.
Bibliografia
[1] M.A. Yahya, Z. Al.-Qodah, C.W. Zanariah Hgah, Renew. Sust. Energy Rev. 2015, 46, 218. [2] P. Gonzalez-Garcia, Renew. Sust. Energy Rev. 2018, 82, 1393. [3] V.M. Mukhin, N.L. Voropaeva, A.G. Tkachev, N.I. Bogdanovich, J.J. Spiridonov, Inżynieria Mineralna 2016, 17, nr 2, 241. [4] M.J. Antal Jr., S.R. Wade, T. Nunoura, J. Anal. Appl. Pyrolysis 2007, 79, 86. [5] A. Bazan, P. Nowicki, R. Pietrzak, Inż. Ochr. Środowiska 2016, 19, nr 2, 183. [6] E. Lorenc-Grabowska, P. Rutkowski, Inż. Ochr. Środowiska 2013, 16, nr 2, 2005. [7] B. Buczek, U. Kanik, Przem. Chem. 2015, 94, nr 12, 2180. [8] W.M. Lewandowski, E. Radziemska, M. Ryms, P. Ostrowski, Proc. ECOpole 2010, 4, nr 2, 453. [9] J. Choma, M. Kloske, Ochr. Środowiska 1999, 73, nr 2, 3. [10] J. Jaramillo, P.M. Alvarez, V. Gomez-Serrano, Fuel Process. Technol. 2010, 91, 1768. [11] J.L. Figueiredo, M.F.R. Pereira, M.M.A. Freitas, J.J.M. Orfao, Carbon 1999, 37, 1379. [12] J.L. Figueiredo, M.F.R. Pereira, Catal. Today 2010, 150, 2. [13] J.J. Jansen, H. van Bekkum, Carbon 1994, 32, 1507. [14] E. Okoniewska, Proc. ECOpole 2014, 8, nr 1, 249. [15] A. Kobyłka, Technical Issues 2016, 4, 27. [16] W. Chwiałkowski, Inż. Ochr. Środowiska 2016, 16, nr 3, 361. [17] J. Kaleta, M. Kida, P. Koszelnik, D. Papciak, A. Puszkarewicz, B. Tchórzewska-Cieślak, Arch. Environ. Prot. 2017, 43, nr 3, 32. [18] A. Deryło-Marczewska, A. Świątkowski, S. Biniak, M. Walczyk, Colloids Surf. A. Physicochem. Eng. Asp. 2008, 327, 1. [19] J. Lach, E. Ociepa, Ochr. Środowiska 2003, 25, nr 3, 57. [20] M. Hofman, R. Pietrzak, Przem. Chem. 2012, 91, nr 12, 2461.
Zeszyt
PRZEMYSŁ CHEMICZNY - e-zeszyt (pdf) 2018-8
licencja: Osobista
Produkt cyfrowy
55.00 zł
Do koszyka
Prenumerata
PRZEMYSŁ CHEMICZNY - prenumerata cyfrowa
licencja: Osobista
Produkt cyfrowy
Nowość
762.00 zł
Do koszyka
PRZEMYSŁ CHEMICZNY - prenumerata PLUS
licencja: Osobista
Szczegóły pakietu
Nazwa
PRZEMYSŁ CHEMICZNY - PAKIET prenumerata PLUS
1002.00 zł brutto
927.78 zł netto
74.22 zł VAT
(stawka VAT 8%)
1002.00 zł
Do koszyka
PRZEMYSŁ CHEMICZNY - papierowa prenumerata roczna + wysyłka
licencja: Osobista
Szczegóły pakietu
Nazwa
PRZEMYSŁ CHEMICZNY - papierowa prenumerata roczna
960.00 zł brutto
888.89 zł netto
71.11 zł VAT
(stawka VAT 8%)
PRZEMYSŁ CHEMICZNY - pakowanie i wysyłka
42.00 zł brutto
34.15 zł netto
7.85 zł VAT
(stawka VAT 23%)
1002.00 zł
Do koszyka
Open Access
Zeszyt
2018-8
Czasopisma
ATEST - OCHRONA PRACY
AURA
AUTO MOTO SERWIS
CHEMIK
CHŁODNICTWO
CIEPŁOWNICTWO, OGRZEWNICTWO, WENTYLACJA
DOZÓR TECHNICZNY
ELEKTROINSTALATOR
ELEKTRONIKA - KONSTRUKCJE, TECHNOLOGIE, ZASTOSOWANIA
GAZETA CUKROWNICZA
GAZ, WODA I TECHNIKA SANITARNA
GOSPODARKA MIĘSNA
GOSPODARKA WODNA
HUTNIK - WIADOMOŚCI HUTNICZE
INŻYNIERIA MATERIAŁOWA
MASZYNY, TECHNOLOGIE, MATERIAŁY - TECHNIKA ZAGRANICZNA
MATERIAŁY BUDOWLANE
OCHRONA PRZED KOROZJĄ
ODZIEŻ
OPAKOWANIE
PACKAGING REVIEW
POLISH TECHNICAL REVIEW
PROBLEMY JAKOŚCI
PRZEGLĄD ELEKTROTECHNICZNY
PRZEGLĄD GASTRONOMICZNY
PRZEGLĄD GEODEZYJNY
PRZEGLĄD MECHANICZNY
PRZEGLĄD PAPIERNICZY
PRZEGLĄD PIEKARSKI I CUKIERNICZY
PRZEGLĄD TECHNICZNY. GAZETA INŻYNIERSKA
PRZEGLĄD TELEKOMUNIKACYJNY - WIADOMOŚCI TELEKOMUNIKACYJNE
PRZEGLĄD WŁÓKIENNICZY - WŁÓKNO, ODZIEŻ, SKÓRA
PRZEGLĄD ZBOŻOWO-MŁYNARSKI
PRZEMYSŁ CHEMICZNY
PRZEMYSŁ FERMENTACYJNY I OWOCOWO-WARZYWNY
PRZEMYSŁ SPOŻYWCZY
RUDY I METALE NIEŻELAZNE
SZKŁO I CERAMIKA
TECHNOLOGIA I AUTOMATYZACJA MONTAŻU
WIADOMOŚCI ELEKTROTECHNICZNE
WOKÓŁ PŁYTEK CERAMICZNYCH