Czasopisma
Czasopisma
Czasopisma
ATEST - OCHRONA PRACY
ATEST - OCHRONA PRACY
AURA
AURA
AUTO MOTO SERWIS
AUTO MOTO SERWIS
CHEMIK
CHEMIK
CHŁODNICTWO
CHŁODNICTWO
CIEPŁOWNICTWO, OGRZEWNICTWO, WENTYLACJA
CIEPŁOWNICTWO, OGRZEWNICTWO, WENTYLACJA
DOZÓR TECHNICZNY
DOZÓR TECHNICZNY
ELEKTROINSTALATOR
ELEKTROINSTALATOR
ELEKTRONIKA - KONSTRUKCJE, TECHNOLOGIE, ZASTOSOWANIA
ELEKTRONIKA - KONSTRUKCJE, TECHNOLOGIE, ZASTOSOWANIA
Czasopisma
Czasopisma
Czasopisma
GAZETA CUKROWNICZA
GAZETA CUKROWNICZA
GAZ, WODA I TECHNIKA SANITARNA
GAZ, WODA I TECHNIKA SANITARNA
GOSPODARKA MIĘSNA
GOSPODARKA MIĘSNA
GOSPODARKA WODNA
GOSPODARKA WODNA
HUTNIK - WIADOMOŚCI HUTNICZE
HUTNIK - WIADOMOŚCI HUTNICZE
INŻYNIERIA MATERIAŁOWA
INŻYNIERIA MATERIAŁOWA
MASZYNY, TECHNOLOGIE, MATERIAŁY - TECHNIKA ZAGRANICZNA
MASZYNY, TECHNOLOGIE, MATERIAŁY - TECHNIKA ZAGRANICZNA
MATERIAŁY BUDOWLANE
MATERIAŁY BUDOWLANE
OCHRONA PRZED KOROZJĄ
OCHRONA PRZED KOROZJĄ
ODZIEŻ
ODZIEŻ
Czasopisma
Czasopisma
Czasopisma
OPAKOWANIE
OPAKOWANIE
PACKAGING REVIEW
PACKAGING REVIEW
POLISH TECHNICAL REVIEW
POLISH TECHNICAL REVIEW
PROBLEMY JAKOŚCI
PROBLEMY JAKOŚCI
PRZEGLĄD ELEKTROTECHNICZNY
PRZEGLĄD ELEKTROTECHNICZNY
PRZEGLĄD GASTRONOMICZNY
PRZEGLĄD GASTRONOMICZNY
PRZEGLĄD GEODEZYJNY
PRZEGLĄD GEODEZYJNY
PRZEGLĄD MECHANICZNY
PRZEGLĄD MECHANICZNY
PRZEGLĄD PAPIERNICZY
PRZEGLĄD PAPIERNICZY
PRZEGLĄD PIEKARSKI I CUKIERNICZY
PRZEGLĄD PIEKARSKI I CUKIERNICZY
Czasopisma
Czasopisma
Czasopisma
PRZEGLĄD TECHNICZNY. GAZETA INŻYNIERSKA
PRZEGLĄD TECHNICZNY. GAZETA INŻYNIERSKA
PRZEGLĄD TELEKOMUNIKACYJNY - WIADOMOŚCI TELEKOMUNIKACYJNE
PRZEGLĄD TELEKOMUNIKACYJNY - WIADOMOŚCI TELEKOMUNIKACYJNE
PRZEGLĄD WŁÓKIENNICZY - WŁÓKNO, ODZIEŻ, SKÓRA
PRZEGLĄD WŁÓKIENNICZY - WŁÓKNO, ODZIEŻ, SKÓRA
PRZEGLĄD ZBOŻOWO-MŁYNARSKI
PRZEGLĄD ZBOŻOWO-MŁYNARSKI
PRZEMYSŁ CHEMICZNY
PRZEMYSŁ CHEMICZNY
PRZEMYSŁ FERMENTACYJNY I OWOCOWO-WARZYWNY
PRZEMYSŁ FERMENTACYJNY I OWOCOWO-WARZYWNY
PRZEMYSŁ SPOŻYWCZY
PRZEMYSŁ SPOŻYWCZY
RUDY I METALE NIEŻELAZNE
RUDY I METALE NIEŻELAZNE
SZKŁO I CERAMIKA
SZKŁO I CERAMIKA
TECHNOLOGIA I AUTOMATYZACJA MONTAŻU
TECHNOLOGIA I AUTOMATYZACJA MONTAŻU
WIADOMOŚCI ELEKTROTECHNICZNE
WIADOMOŚCI ELEKTROTECHNICZNE
WOKÓŁ PŁYTEK CERAMICZNYCH
WOKÓŁ PŁYTEK CERAMICZNYCH
Menu
Menu
Menu
Prenumerata
Prenumerata
Publikacje
Publikacje
Drukarnia
Drukarnia
Kolportaż
Kolportaż
Reklama
Reklama
O nas
O nas
ui-button
Twój Koszyk
Twój koszyk jest pusty.
Niezalogowany
Niezalogowany
Zaloguj się
Zarejestruj się
Reset hasła
Czasopismo
|
HUTNIK - WIADOMOŚCI HUTNICZE
|
Rocznik 2015 - zeszyt 8
Określenie morfologii mikrostruktury stali perlitycznej walcowanej na gorąco
10.15199/24.2015.8.7
Janusz SZALA
Dariusz KUC
nr katalogowy: 92855
10.15199/24.2015.8.7
W artykule przedstawiono metodykę ilościowego opisu morfologii perlitu w stalach, na której bazuje nowy program komputerowy "PILS" - Pearlite Inter-Lamellar Spacing. W ramach weryfikacji przeprowadzono badania ilościowe mikrostruktury próbek po symulacji fizycznej obróbki cieplno-plastycznej na dylatometrze odkształceniowym ze zróżnicowaną szybkością chłodzenia dla stali C70D. Wykonano ponadto pomiary dla próbek walcówki uzyskanej w warunkach przemysłowych według obecnie stosowanej technologii. Opracowany program i przeprowadzone badania będą wykorzystane przy pracach nad opracowaniem zmodyfikowanej technologii walcowania walcówki, dla uzyskania wyrobów ze stali, których mikrostruktura charakteryzuje się mniejszą odległością międzypłytkową - poniżej 0,2 mikro m. The article presents the methodology of quantitative description of pearlite morphology in steels with the use of the method which a new computer program "PILS" - Pearlite Inter-Lamellar Spacing is based on. In order to verify the method, some quantitative tests of microstructure in samples after physical simulation of heat-plastic treatment were conducted on a deformation dilatometer device with diverse cooling speed for steel C70D. Moreover, measurements were conducted for samples of wire rod prepared in industrial conditions according to currently applied technologies. Elaborated program and conducted tests will be used during preparations of modified technologies of wire rod rolling to prepare products made of steel, the microstructure of which is characterised with smaller interlamellar spacing - below 0.2 mikro m. Słowa kluczowe: mikrostruktura, metalografia ilościowa, odległość międzypłytkowa, symulacja fizyczna Key words: microstructure, quantitative metallography, interlamellar spacing, physical simulation.Wprowadzenie. Szereg właściwości mechanicznych stali perlitycznych zależy od stopnia dyspersji perlitu. Podstawowym parametrem stereologicznym stosowanym do opisu t[...]
Treść płatna
Jeśli masz wykupiony/przyznany dostęp -
zaloguj się
.
Skorzystaj z naszych propozycji zakupu!
Publikacja
e-Publikacja (format pdf) - nr 92855 "Określenie morfologii mik..."
licencja: Osobista
Produkt cyfrowy
10.00 zł
Do koszyka
Zeszyt
HUTNIK - WIADOMOŚCI HUTNICZE - e-zeszyt (pdf) 2015-8
licencja: Osobista
Produkt cyfrowy
32.00 zł
Do koszyka
Prenumerata
HUTNIK - WIADOMOŚCI HUTNICZE - prenumerata cyfrowa
licencja: Osobista
Produkt cyfrowy
Nowość
400.00 zł
Do koszyka
HUTNIK - WIADOMOŚCI HUTNICZE - papierowa prenumerata roczna + wysyłka
licencja: Osobista
Szczegóły pakietu
Nazwa
HUTNIK - WIADOMOŚCI HUTNICZE - papierowa prenumerata roczna
540.00 zł brutto
500.00 zł netto
40.00 zł VAT
(stawka VAT 8%)
HUTNIK - WIADOMOŚCI HUTNICZE - pakowanie i wysyłka
14.00 zł brutto
11.38 zł netto
2.62 zł VAT
(stawka VAT 23%)
554.00 zł
Do koszyka
HUTNIK - WIADOMOŚCI HUTNICZE - PAKIET prenumerata PLUS
licencja: Osobista
Szczegóły pakietu
Nazwa
HUTNIK - WIADOMOŚCI HUTNICZE - PAKIET prenumerata PLUS
600.00 zł brutto
555.56 zł netto
44.44 zł VAT
(stawka VAT 8%)
600.00 zł
Do koszyka
Zeszyt
2015-8
Czasopisma
ATEST - OCHRONA PRACY
AURA
AUTO MOTO SERWIS
CHEMIK
CHŁODNICTWO
CIEPŁOWNICTWO, OGRZEWNICTWO, WENTYLACJA
DOZÓR TECHNICZNY
ELEKTROINSTALATOR
ELEKTRONIKA - KONSTRUKCJE, TECHNOLOGIE, ZASTOSOWANIA
GAZETA CUKROWNICZA
GAZ, WODA I TECHNIKA SANITARNA
GOSPODARKA MIĘSNA
GOSPODARKA WODNA
HUTNIK - WIADOMOŚCI HUTNICZE
INŻYNIERIA MATERIAŁOWA
MASZYNY, TECHNOLOGIE, MATERIAŁY - TECHNIKA ZAGRANICZNA
MATERIAŁY BUDOWLANE
OCHRONA PRZED KOROZJĄ
ODZIEŻ
OPAKOWANIE
PACKAGING REVIEW
POLISH TECHNICAL REVIEW
PROBLEMY JAKOŚCI
PRZEGLĄD ELEKTROTECHNICZNY
PRZEGLĄD GASTRONOMICZNY
PRZEGLĄD GEODEZYJNY
PRZEGLĄD MECHANICZNY
PRZEGLĄD PAPIERNICZY
PRZEGLĄD PIEKARSKI I CUKIERNICZY
PRZEGLĄD TECHNICZNY. GAZETA INŻYNIERSKA
PRZEGLĄD TELEKOMUNIKACYJNY - WIADOMOŚCI TELEKOMUNIKACYJNE
PRZEGLĄD WŁÓKIENNICZY - WŁÓKNO, ODZIEŻ, SKÓRA
PRZEGLĄD ZBOŻOWO-MŁYNARSKI
PRZEMYSŁ CHEMICZNY
PRZEMYSŁ FERMENTACYJNY I OWOCOWO-WARZYWNY
PRZEMYSŁ SPOŻYWCZY
RUDY I METALE NIEŻELAZNE
SZKŁO I CERAMIKA
TECHNOLOGIA I AUTOMATYZACJA MONTAŻU
WIADOMOŚCI ELEKTROTECHNICZNE
WOKÓŁ PŁYTEK CERAMICZNYCH